Alloy Digest (1955) 4 (6): CS-3.
Published: 01 June 1955
... MAX-EL 1-B offers a case hardening grade of excellent machining characteristics, plus good mechanical properties in the core with minimum distortion during heat treatment. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1961) 10 (4): CS-15.
Published: 01 April 1961
... Max-EL 2-B is a general purpose free-machining steel offering a good combination of strength, toughness and abrasion resistance, as well as excellent machinability. It is generally used in the as-rolled condition at a Brinell hardness of 200-235. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1993) 42 (2): Ti-104.
Published: 01 February 1993
... (lO-VC *8.12 + 8.17 x 1O-3 (T) -1.37x10-2~+1x1O-s 03 Special heat (cal/gm C) Resistivity (lo-8 ohm-m) Conductivity (W/M*K) *WhereT=OC *.117+6.7xl~(T) * 178 + .057 (I ) -5 x lo-SC132 * 6.62 + 1.27 x 1O-2 (T) Residual Elements, Total 0.30 Max PROPERTIES Table 1 - TYPICAL TENSILE PROPERTIES. Beta Forned...
Journal Articles
Alloy Digest (1985) 34 (7): SA-410.
Published: 01 July 1985
....* 0.025 max.* 0.15-O. 35 0.75-l. 10 0. I 5-O. 25 0.0005 min. Physical Constants: (Approximate) Density, lb/cu in. 0.283 Specific gravity 7.83 Specific heat, Btu/lb/ OF (120-210°F) 0.115 Thermal coef. expansion / O F (70- 1000 F) 7.3 x 10-b Thermal conductivity, Btu I ft / in. / hr / OF (O-200 F) 225...
Journal Articles
Alloy Digest (1986) 35 (10): Al-272.
Published: 01 October 1986
... T61 Temper TSS 1 Temper T65 Temper Tcn\ilc rtrcnpth, psi Ylcld Strength (0.2 offwt). pst Elong;llion (2 in %. Brincll h;lrdnc\s (SfH~/l0/30) Shear htrcngth. p\i I:ati;uc <lrcn;lth (5 s 108 qclcx). psi Comprcwvc yield \trcnfth, p\~ 2700(, 41000 37000 48000 20000 40000 35000 36000 I .o 0.5 max. 0.5 max...
Journal Articles
Alloy Digest (2001) 50 (6): Ni-568.
Published: 01 June 2001
... (Nickel Alloy) Filing Code: Ni-568 Nickel June 2001 NICROFER® 7216LC Chemical Composition, wt Carbon 0.025 max Manganese 1.0 max Silicon 0.05 max Nickel 72.0 min Chromium 14.0 17.0 Copper 0.5 max Phosphorus 0.3 max Sulfur 0.010 max Iron 6.0 10.0 Aluminum 0.3 max Boron 0.006 max Physical Properties...
Journal Articles
Alloy Digest (1972) 21 (9): Ti-67.
Published: 01 September 1972
... resistivity, microhm-cm Specific heat, Btu/lb/oF Modulus of elasticity, psi (tension) Modulus of rigidity, psi Ti-75A Ti- 1 OOA 0.05 max 0.08 max 0.05 max 0.05 max 0.015 max - 0.0 125 max 0.0125 max 0.0100 max 0.010 max 0.30 max 0.30 max Remainder Remainder Ti-75A Ti- 1 OOA 0.164 0.164 3020 3025 4.8 x 10-6...
Journal Articles
Alloy Digest (1991) 40 (10): Al-320.
Published: 01 October 1991
... Equivalents: ASME: SB 210, drawn seamless tubing SB 221, extruded wire, rod, bar, shapes and tube SB 241, pipe and tube ASTM: B 210, drawn seamless tubing B 22 1, extruded wire, rod, bar, shapes and tube B 241, seamless extruded pipe and tube B 345, pipe for gas and oil transmission B 429, extruded structural...
Journal Articles
Alloy Digest (2002) 51 (12): Al-383.
Published: 01 December 2002
... max Others, total 0.15 max Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3 ) 2740 (0.099) Melting range, approximate, °C (°F) 520 585 (970 1085) Anodize color Gray Weldability: Typical procedures are given in Table 1. The alloy is widely pre- ferred by welders because of its wetting ability...
Journal Articles
Alloy Digest (2011) 60 (10): CS-167.
Published: 01 October 2011
... strength, R p0.2 or R eL , min max, MPa (ksi) Tensile strength, R m , min max, MPa (ksi) Elongation(b), A 80 , min, % Inside radius for 90° bend, (t=thickness) Dogal 300 LAD 300 380 (44 55) 380 480 (55 70) 23 0.75*t Dogal 340 LAD 340 420 (49 61) 410 510 (59 74) 21 0.75*t Dogal 380 LAD 380 480 (55 70) 440...
Journal Articles
Alloy Digest (1986) 35 (10): Ni-341.
Published: 01 October 1986
... is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor ele- ments are controlled to provide increased resistance to weld heat-affected zone corrosion. The alloy has exceptional stress-corrosion cracking resistance in chloride-containing environments. *INCO is a trademark...
Journal Articles
Alloy Digest (2002) 51 (2): SS-845.
Published: 01 February 2002
... 0.20 0.40 Titanium 0.20 0.50 Al + Ti 0.7 max Phosphorus 0.015 max Sulfur 0.010 max Iron bal Physical Properties: Density, kg/m3 (lb/in.3 ) 8000 (0.29) Melting range, °C (°F) 1350 1400 (2460 2550) Permeability at 20 °C (68 °F) 1.01 See also Table 1. Mechanical Properties: (Minimum at room temperature...
Journal Articles
Alloy Digest (1962) 11 (12): Cu-123.
Published: 01 December 1962
... 50 Teosile Yield Streog th Strength psi psi (0.5%) 66000 29000 77000 43000 87000 51000 94000 55000 99000 54000 101000 51000 Elongation % in 2 36 24 16 10 8 7.5 Rockwell Hardness B Table 3 - EFFECT OF ANNEALING - Rod (Rod nreviouslv cold worked 30% reduction of area) Annealing Tensile Temperature...
Journal Articles
Alloy Digest (2005) 54 (9): SS-938.
Published: 01 September 2005
... ±0.030 0.120 ±10 Ovality allowance to ASTM A 269. Straightness 0.030 in. max per 3 ft length. Lengths 20 ft minus 0 in. plus 2 in. (a) Other wall thicknesses available upon request. (b) Six in. available in a 20 µin. (0.50 µm) Ra finish ...
Journal Articles
Alloy Digest (1999) 48 (8): SS-757.
Published: 01 August 1999
... worked conditions for 25 mm (1 in.) bar and 2.5 mm (0.1 in.) wire. Toughness and Ductile-to-Brittle Transition. Like most austenitic alloys, BioDur 108 alloy has very high toughness lev- els. In the annealed condition, room-temperature impact-energy levels for standard 10 mm by 10 mm Charpy V-notch...
Journal Articles
Alloy Digest (1993) 42 (6): SS-546.
Published: 01 June 1993
... 4.5 0.10 0.30 Bal. PROPERTIES Table 1 - PHYSlCAL PROPERTIES pRcm acirc mil ft 029 (79) 2430-2520 (1330-1380) cl.01 See Table 1 See Table 1 See Table 1 See Table 1 See Table 1 Modulus of Elasticity kN/mn? ldksi Coefficient of thennalexpansion b&?tWeCll roomteJnpaamrc *O%and*~pF 15.5 - 16.6 9 17.0 3 ii...
Journal Articles
Alloy Digest (1997) 46 (7): SA-485.
Published: 01 July 1997
... Composition, wt -a) w-a z 0.17lnaL 0.90-150 pt w 0.020 max. Et 0.020 Nax. 0.15460 NIJ;el . . . . . . l-w . . . Vanadhrm . . . E-z . . . . . . FCM 030 CE . . . (a) lLpiral unkss noted diffemdy wddaby1w W-W 0.14 0.17 1.29 0.86 0.006 0.007 0.004 0.003 0.39 0.23 . . . 0.86 . . . 053 0.16 053 . . . 056...
Journal Articles
Alloy Digest (1998) 47 (8): Al-351.
Published: 01 August 1998
.... The use of a chip breaker is suggested. The ahoy is rated B on the Aluminum Association machinability rating system, giving Table 1 Typical Mechanical Properties TensiIe~ Yield strength Elongncion in Temper MPa ksi MPa ksi Lia% T65l.coldh 309 45 175 40 17 ished T8.coldfinkhed 351 51 337 49 I5 T9. cold...
Journal Articles
Alloy Digest (1999) 48 (2): Al-358.
Published: 01 February 1999
... an ele- vated temperature shaping process. These products can reduce minor straightening after stretching to comply with standard tol- erances. Aging treatment is 190 °C (275 °F) for 18 h. Weldability: This alloy can be welded with proper procedure and equipment. Because of the effect of heating...
Journal Articles
Alloy Digest (1980) 29 (11): SA-378.
Published: 01 November 1980
... for the construction of equipment to operate at temperatures as low as -9OOF. It is intended primarily for welded pressure vessels. Composition: (Heat Analysis) Physical Constants: Carbon Manganese Phosphorus SlllfllI Silicon Nickel Iron Grade A Grade B 0.17 max* 0.70 max* 0.035 max. 0.040 max. 0.15-0.40 2.10-2.50...