... MAR-M alloy 246 is a vacuum-cast nickel-base alloy combining precipitation hardening and solid solution strengthening. It has high rupture strength and adequate ductility in the recommended operating temperature range of 1200-1900 F. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2013) 62 (9): SA-682.
Published: 01 September 2013
... www.asminternational.org Filing Code: Steel Alloy September 2013 SA-682 MARS 270 is a high hardness (510/550 HB) steel for ballistic protection. MARS® 270 (Armor Steel) MARS® 270 Chemical Composition, wt (Typical values, maximum) Carbon 0.4 Chromium 1.5 Nickel 4.0 Molybdenum 0.6 Manganese 1.2 Sulfur 0.002 Phosphorus 0.010...
Journal Articles
Alloy Digest (2023) 72 (8): CS-257.
Published: 01 August 2023
... °C (390 °F): tempered martensite, well- defined acicular structure. (b) 400 °C (750 °F): tempered mar- tensite, acicular structure less defined due to the changes happening during tempering. Source: Ref 41 (p 329) Table 10 Recommended ranges of nitriding potential for non-alloy steels Class 0 1 2...
Journal Articles
Alloy Digest (2023) 72 (5): CS-247.
Published: 01 May 2023
... = 0.67%. (b) Specimen size: Disks are 20 mm (0.8 in.) diameter × 60 mm (2.4 in.) long. (c) Heat treatment: Quenched in water at 30 °C (85 °F); agitation by upward nozzle jet (1 m/s, or 3 ft/s). Source: Ref 23 (p 114) Alloy Digest: Data on Worldwide Metals and Alloys CS-247 / 10 Fig. 18 Effect of mass...