Alloy Digest (1984) 33 (2): Ni-291.
Published: 01 February 1984
... MAGNIFER 7904 is a soft magnetic nickel-iron alloy containing about 5% molybdenum. It offers extremely high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound troids, laminations, shielding and relay parts. This datasheet provides...
Journal Articles
Alloy Digest (2001) 50 (12): Fe-123.
Published: 01 December 2001
... measuring temperature for Magnifer 4008 compared with the 80% Ni alloy Magnifer 7904. Fig. 5 Mean coefficient of thermal expansion, AK, between 20 °C (68 °F) and the respective temperature following heat treatment for 15 min at 950 °C (1740 °F). Fig. 2 DC permeability of Magnifer 4008 in relation to field...