Alloy Digest (1966) 15 (1): Cu-159.
Published: 01 January 1966
... Lumen 97 is a heat treatable aluminum bronze having high hardness coupled with sufficient ductility suitable for gears, bushings and bearings subjected to heavy pressures and excessive wear. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...