Skip Nav Destination
Close Modal
Search Results for
Lucefin Group 37CrS4
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Lucefin Group 37CrS4
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2020) 69 (5): SA-862.
Published: 01 May 2020
... Lucefin Group 37Cr4 and 37CrS4 are medium-carbon, 1% chromium, direct hardening alloy steels that are also suitable for flame and induction hardening. These steels are low hardenability steels in the 0.30 to 0.37 mean carbon content classification. They are used for water-quenched parts...
Abstract
View article
PDF
Lucefin Group 37Cr4 and 37CrS4 are medium-carbon, 1% chromium, direct hardening alloy steels that are also suitable for flame and induction hardening. These steels are low hardenability steels in the 0.30 to 0.37 mean carbon content classification. They are used for water-quenched parts of moderate section size and for oil-quenched parts of small section size. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as forming, machining, and joining. Filing Code: SA-862. Producer or source: Lucefin S.p.A.