Alloy Digest (2021) 70 (7): CS-211.
Published: 01 July 2021
... Lucefin C25, C25E, and C25R are low-carbon, non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. These steels are typically used for small, moderately stressed parts, where higher strength levels are needed than can be achieved in the lower carbon...