Alloy Digest (1952) 1 (1): TS-1.
Published: 01 September 1952
... Latrobe BR-4 is a high-vanadium, high-chromium tool and die steel of the air hardening and nondeforming type. In the hardened condition it is extremely abrasion resistant. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1986) 35 (7): TS-460.
Published: 01 July 1986
... on forming, heat treating, and machining. Filing Code: TS-460. Producer or source: Latrobe Steel Company. Producer or Source: Latrobe Steel Company Copyright © ASM International® 1996 1996 ASM International abrasion resistance BR-4 DIE STEEL chemical composition elasticity fracture toughness...