1-2 of 2 Search Results for

LUKENS HARDWEAR 400

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1994) 43 (2): SA-470.
Published: 01 February 1994
... LUKENS HARDWEAR 400 is a premium abrasion resistant alloy steel with improved forming and welding characteristics. Typical surface hardness range (BHN) of 321-444, depending on thickness. This datasheet provides information on composition and hardness. It also includes information on forming...
Journal Articles
Alloy Digest (1994) 43 (3): SA-471.
Published: 01 March 1994
... LUKENS HARDWEAR 425 is a premium abrasion resistant alloy steel with improved forming and welding characteristics. Typical surface hardness range (BHN) is 400-444, depending on thickness. This datasheet provides information on composition and hardness. It also includes information on forming...