Alloy Digest (2012) 61 (12): TS-712.
Published: 01 December 2012
... LSS H19 is a hot work tool steel with resistance to softening. This datasheet provides information on composition and physical properties. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-712. Producer or source: Latrobe Specialty Steel...