Alloy Digest (2012) 61 (11): TS-709.
Published: 01 November 2012
... LSS H14 is a hot work tool steel to which tungsten has been added. It is deep hardening. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-709. Producer or source: Latrobe...