Skip Nav Destination
Close Modal
Search Results for
LSS H13 HC
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
LSS H13 HC
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2013) 62 (3): TS-715.
Published: 01 March 2013
... LSS H13 HC is a hot work tool steel that is a high-carbon modification of LSS H13 (Alloy Digest TS-708, October 2012). This version has improved wear resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on wear...
Abstract
View article
PDF
LSS H13 HC is a hot work tool steel that is a high-carbon modification of LSS H13 (Alloy Digest TS-708, October 2012). This version has improved wear resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-715. Producer or source: Latrobe Specialty Steel Company.