Alloy Digest (2010) 59 (7): Ni-680.
Published: 01 July 2010
... Although LSS 718 EP is a premier aerospace nickel-base alloy, it has a significant presence in exploration and production (EP) of oil and gas and this modification is meant for those applications. This datasheet provides information on composition, physical properties, hardness, elasticity...