Alloy Digest (1962) 11 (9): Cu-120.
Published: 01 September 1962
... LOHM is a copper-nickel alloy recommended for resistors where low specific resistance is desired. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Cu-120. Producer or source: Driver-Harris Company. Producer or Source: Driver-Harris...