Alloy Digest (2001) 50 (2): SS-818.
Published: 01 February 2001
... Lescalloy Jethete M-152 ESR is a martensitic stainless steel that is hardenable to product high strength for structural components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat...