Skip Nav Destination
Close Modal
Search Results for
LESCALLOY BG42 VIM-VAR
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Search Results for LESCALLOY BG42 VIM-VAR
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1992) 41 (2): SS-179.
Published: 01 February 1992
... LESCALLOY BG42 VIM-VAR is a martensitic stainless high-speed steel that combines the temper resistance and hot hardness characteristics of M-50 high-speed steel with the corrosion resistance of AISI Type 440C stainless steel. (See also LESCALLOY BG42, Alloy Digest SS-280, October 1972...
Abstract
View articletitled, <span class="search-highlight">LESCALLOY</span> <span class="search-highlight">BG42</span> <span class="search-highlight">VIM</span>-<span class="search-highlight">VAR</span>: High Performance Bearing Steel
View
PDF
for article titled, <span class="search-highlight">LESCALLOY</span> <span class="search-highlight">BG42</span> <span class="search-highlight">VIM</span>-<span class="search-highlight">VAR</span>: High Performance Bearing Steel
LESCALLOY BG42 VIM-VAR is a martensitic stainless high-speed steel that combines the temper resistance and hot hardness characteristics of M-50 high-speed steel with the corrosion resistance of AISI Type 440C stainless steel. (See also LESCALLOY BG42, Alloy Digest SS-280, October 1972.) This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-179. Producer or source: Latrobe Steel Company. Originally published as Lesco BG42, March 1966, revised February 1992. See also Alloy Digest SS-356, October 1978.
Journal Articles
Alloy Digest (1978) 27 (10): SS-356.
Published: 01 October 1978
... LESCALLOY BG42 VIM-VAR combines the tempering, hardness and hardness-retention characteristics of AISI M50 high-speed steel with the corrosion and oxidation resistance of AISI Type 440C stainless steel. LESCALLOY BG42 VIM-VAR is double vacuum melted (VIM, Vacuum Induction Melted; VAR, Vacuum Arc...
Abstract
View articletitled, <span class="search-highlight">LESCALLOY</span> <span class="search-highlight">BG42</span> <span class="search-highlight">VIM</span>-<span class="search-highlight">VAR</span>: Martensitic, Stainless, High-Speed Steel
View
PDF
for article titled, <span class="search-highlight">LESCALLOY</span> <span class="search-highlight">BG42</span> <span class="search-highlight">VIM</span>-<span class="search-highlight">VAR</span>: Martensitic, Stainless, High-Speed Steel
LESCALLOY BG42 VIM-VAR combines the tempering, hardness and hardness-retention characteristics of AISI M50 high-speed steel with the corrosion and oxidation resistance of AISI Type 440C stainless steel. LESCALLOY BG42 VIM-VAR is double vacuum melted (VIM, Vacuum Induction Melted; VAR, Vacuum Arc Remelted) to consistently assure good cleanliness and superior properties. It is used for bearings, gears, ball screws and other aerospace applications. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fatigue. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-356. Producer or source: Latrobe Steel Company. See also Alloy Digest SS-179, revised February 1992.