1-2 of 2 Search Results for

LESCALLOY 4340 VAC-ARC

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (7): SA-361.
Published: 01 July 1979
... LESCALLOY 4340 VAC-ARC is a low-alloy steel that can be heat treated to high strength levels. It has a good combination of strength, ductility and toughness along with high hardenability. It is produced by the vacuum-consumable-electrode process to provide optimum cleanliness and preferred ingot...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (2): SA-343.
Published: 01 February 1978
... LESCALLOY HP 9-4-30 VAC-ARC is a low-alloy, high-strength steel with a high nickel content to promote toughness. It was designated for high hardenability and good weldability. It is produced by the vacuum-consumable-electrode process to insure cleanliness and provide a preferred ingot structure...