Journal Articles
Alloy Digest (1993) 42 (2): SA-321.
Published: 01 February 1993
... LESCALLOY 300M VAC ARC is a low-alloy steel with an excellent combination of high hardenability and high strength coupled with good ductility and good toughness. Its tensile strength ranges from 280,000 to 300,000 psi. It is produced by the vacuum consumable electrode melting process to provide...
Journal Articles
Alloy Digest (2015) 64 (3): SA-722.
Published: 01 March 2015
... Lescalloy 300M-HS VAC-ARC is a clean high-strength, low-alloy steel with high strength, fracture toughness, and hardenability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating...