1-3 of 3 Search Results for

LEHIGH-S

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1962) 11 (6): TS-119.
Published: 01 June 1962
... LEHIGH-S is the oil-hardening type of high-carbon high-chromium tool and die steel, having high abrasion resistance and very little change in size and shape during heat treatment. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1954) 3 (10): TS-26.
Published: 01 October 1954
... Lehigh H is a standard air-hardening type of high-carbon, high-chromium tool steel. It combines maximum abrasion-resistance and fair toughness with a minimum distortion in hardening. It corresponds to SAE Type IID-2 tool steel. This datasheet provides information on composition, hardness...
Journal Articles
Alloy Digest (1957) 6 (3): TS-56.
Published: 01 March 1957
... temperature to insure proper di&tsion of carbides. We suggest a soak- ing time about double that used for a similar size specimen of Carbon Tool Steel. Depth of cut l/32 l/16 $2 RECOMMENDED CU ITING High Speed Steel Feed S d in. /rev. p s pm l/64 5460 i$$ 45-50 8. 43 39 l/32 4146 1/16 33-37 SPEEDS...