Alloy Digest (1997) 46 (11): Al-343.
Published: 01 November 1997
... Lanxide 92-X-2050 is an aluminum-10 Silicon-1 Magnesium-1 Iron alloy with 30 vol.% of silicon carbide particulate. This metal-matrix composite is designed to outperform the unreinforced counterpart. The alloy-matrix composite is available as die castings. This datasheet provides information...