Alloy Digest (1999) 48 (9): SS-761.
Published: 01 September 1999
... Kubota alloy KRH35CL is similar to KHR35C but contains lower carbon for applications requiring good thermal fatigue and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...