Skip Nav Destination
Close Modal
Search Results for
Kubota alloy KHR35C
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-12 of 12 Search Results for
Kubota alloy KHR35C
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1999) 48 (7): SS-753.
Published: 01 July 1999
... Kubota alloy KHR35C is similar to HP alloy with the addition of niobium to increase its creep-rupture strength. Typical applications include components and assemblies for severe carburizing environments, such as ethylene pyrolysis coils. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Kubota alloy KHR35C is similar to HP alloy with the addition of niobium to increase its creep-rupture strength. Typical applications include components and assemblies for severe carburizing environments, such as ethylene pyrolysis coils. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting and joining. Filing Code: SS-753. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (1999) 48 (8): SS-755.
Published: 01 August 1999
... KHR35C Hi Si is similar to Kubota alloy KHR35C but with added silicon levels to improve carburization resistance. The typical application is ethylene furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes...
Abstract
View article
PDF
KHR35C Hi Si is similar to Kubota alloy KHR35C but with added silicon levels to improve carburization resistance. The typical application is ethylene furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting and joining. Filing Code: SS-755. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (1999) 48 (9): SS-761.
Published: 01 September 1999
... Kubota alloy KRH35CL is similar to KHR35C but contains lower carbon for applications requiring good thermal fatigue and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Abstract
View article
PDF
Kubota alloy KRH35CL is similar to KHR35C but contains lower carbon for applications requiring good thermal fatigue and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-761. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (1999) 48 (12): SS-772.
Published: 01 December 1999
... KHR35CW is a further modification of the KHR35C family (see Alloy Digest SS-753, July 1999, and SS-755, August 1999) with additions of tungsten and molybdenum to the 25Cr-36Ni content. These modifications are used primarily to further increase the carburization resistance of the alloy...
Abstract
View article
PDF
KHR35CW is a further modification of the KHR35C family (see Alloy Digest SS-753, July 1999, and SS-755, August 1999) with additions of tungsten and molybdenum to the 25Cr-36Ni content. These modifications are used primarily to further increase the carburization resistance of the alloy. This datasheet provides information on composition and physical properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-772. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (1999) 48 (11): SS-767.
Published: 01 November 1999
... 1999 ASM International cast metal products castability chemical composition creep properties Kubota Alloy KHR 35CT HiSi oxidation resistance physical properties tensile properties thermal properties KUBOTA ALLOY KHR 35CT HiSi (Heat Resistant Alloy) KHR 35 CT HiSi is a modification...
Abstract
View article
PDF
KHR 35CT HiSi is a modification of KHR 35C HiSi (see Alloy Digest SS-753, July 1999, and SS-755, August 1999) by the addition of both silicon and titanium as the microalloying additions. The strength, oxidation resistance, and metal dusting resistance improve its use for ethylene pyrolysis coils. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting. Filing Code: SS-767. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (2001) 50 (4): Ni-564.
Published: 01 April 2001
... 1000 °C (70 1832 °F) 16.6 (9.2) Mechanical Properties: See Tables 1 and 2. Weldability: Procedures for welding KHR35H are available from Kubota Metal Corporation. General Characteristics: KHR35H is a 25Cr-35Ni-Fe base alloy modified by an addition of molybdenum to increase creep and rupture strength...
Abstract
View article
PDF
KHR35H is a high-temperature heat resistant alloy with a molybdenum addition to increase creep and rupture strength to levels better than those of HP alloy. Typical applications are in heat treatment equipment. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-564. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (2001) 50 (7): Ni-570.
Published: 01 July 2001
...-chromium alloy de- veloped for ethylene pyrolysis service at temperatures up to 1130 °C (2066 °F). Carburization resistance is significantly higher than the HP-modified alloys, while creep strength is greater than that of KHR35C Hi Si. KHR45A is Kubota s pre- miere material for ethylene pyrolysis furnaces...
Abstract
View article
PDF
KHR45A is a niobium-containing Ni-Cr-Fe alloy with very high temperature usage and high caburization resistance. It is typically used in pyrolysis tubes and fittings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as joining. Filing Code: Ni-570. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (2001) 50 (6): Ni-567.
Published: 01 June 2001
... as creep. It also includes information on corrosion resistance. Filing Code: Ni-567. Producer or source: Kubota Metal Corporation. Producer or Source: Kubota Metal Corporation Copyright © ASM International® 2001 2001 ASM International cast nickel alloys chemical composition corrosion...
Abstract
View article
PDF
KHR35H-HiSi is an improvement over HP alloy in oxidation resistance and creep strength. This composition also has high silicon for resisting carburizing environments in ethylene pyrolysis coils. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on corrosion resistance. Filing Code: Ni-567. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (2001) 50 (8): Ni-571.
Published: 01 August 2001
... Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570, July 2001) that changes either ductility or carburization resistance. The typical application is as outlet tubes and fittings in pyrolysis service. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570, July 2001) that changes either ductility or carburization resistance. The typical application is as outlet tubes and fittings in pyrolysis service. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance, and corrosion resistance. Filing Code: Ni-571. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (2002) 51 (6): Ni-585.
Published: 01 June 2002
... KUBOTA KHR48N HiSi is a Ni-Cr-Fe alloy with a 5% W addition. The alloy was designed for high-temperature operating parameters of strength, good carburization resistance, and high oxidation resistance. It is a modification of KHR48N (see Alloy Digest Ni-582, May 2002) adjusted in composition...
Abstract
View article
PDF
KUBOTA KHR48N HiSi is a Ni-Cr-Fe alloy with a 5% W addition. The alloy was designed for high-temperature operating parameters of strength, good carburization resistance, and high oxidation resistance. It is a modification of KHR48N (see Alloy Digest Ni-582, May 2002) adjusted in composition to maximize carburization resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as joining. Filing Code: Ni-585. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
Alloy Digest (2002) 51 (5): Ni-582.
Published: 01 May 2002
... KUBOTA KHR48N is a Ni-Cr-Fe-W high-carbon alloy with high-temperature operating parameters of strength, good carburization resistance, and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes...
Abstract
View article
PDF
KUBOTA KHR48N is a Ni-Cr-Fe-W high-carbon alloy with high-temperature operating parameters of strength, good carburization resistance, and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as joining. Filing Code: Ni-582. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
Alloy Digest (2001) 50 (9): Ni-573.
Published: 01 September 2001
... Kubota KHR35W has additions of tungsten to 25Cr-35Ni base alloy (Alloy digest SS-755, August 1999). The tungsten is used to further increase carburization resistance in service at temperatures up to 1095 C (2000 F). This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Kubota KHR35W has additions of tungsten to 25Cr-35Ni base alloy (Alloy digest SS-755, August 1999). The tungsten is used to further increase carburization resistance in service at temperatures up to 1095 C (2000 F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-573. Producer or source: Kubota Metal Corporation.