Alloy Digest (2012) 61 (1): SS-1112.
Published: 01 January 2012
... Kubota Alloy HE is a heat-resisting stainless steel casting suitable for long-term service at temperatures up to 1095 C (2000 F). This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2011) 60 (12): SS-1110.
Published: 01 December 2011
... Kubota Alloy HD (UNS J93005) is a heat-resisting stainless steel casting alloy suitable for long-term service at temperatures up to 1095 deg C (2000 deg F). The nearest wrought equivalent is type 327. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2012) 61 (2): SS-1115.
Published: 01 February 2012
... Kubota Alloy HF is a heat-resisting stainless steel casting suitable for long-term service at temperatures between 538-871 deg C (1000-1600 deg F). It is frequently used as an alternative to the 2.25%Cr-1%Mo steels due to its greater ease of fabrication. This datasheet provides information on...
Journal Articles
Alloy Digest (2010) 59 (2): SS-1052.
Published: 01 February 2010
... Kubota Alloy HI is a heat-resistant stainless steel casting suitable for long-term service at temperatures up to 1105 deg C (2025 deg F). Furnace skids and rail, conveyor roll assemblies, lead pots and retorts are typical applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2010) 59 (5): SS-1065.
Published: 01 May 2010
... Kubota Alloy HC is a heat resisting stainless steel casting suitable for long term service at temperatures up to 1093 deg C (2000 deg F). This alloy can maintain resistance to sulfur bearing environments up to 1093 deg C (2000 deg F). This datasheet provides information on composition, physical...