Alloy Digest (1985) 34 (12): Fe-71.
Published: 01 December 1985
... KANTHAL AF is an Fe-Cr-Al alloy intended for heating elements with element temperatures up to 1400 C. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: Fe-71. Producer or source: The Kanthal Corporation. Producer or Source...
Journal Articles
Alloy Digest (1997) 46 (8): SS-694.
Published: 01 August 1997
... Kanthal APM is an electric resistance heating alloy based on the iron-chromium-aluminum family. Alloys of this family have longer lives and higher operating temperatures than nickel-chromium alloys. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1967) 16 (12): SS-203.
Published: 01 December 1967
... KANTHAL-DS is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns up to 2335 F. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1970) 19 (5): SS-238.
Published: 01 May 1970
... Kanthal A-1 is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. Maximum operating temperature 2505 F (1375 C). This datasheet provides information on composition...
Journal Articles
Alloy Digest (1954) 3 (7): SS-16.
Published: 01 July 1954
... KANTHAL-A is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1955) 4 (9): SS-34.
Published: 01 September 1955
... KANTHAL-D is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2008) 57 (8): Mn-5.
Published: 01 August 2008
... Kanthal 200 R 110 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: MN-5...
Journal Articles
Alloy Digest (2008) 57 (10): Fe-147.
Published: 01 October 2008
... Kanthal 155 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 350 deg C, −4 to 660 deg F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code...
Journal Articles
Alloy Digest (2009) 58 (6): SS-1037.
Published: 01 June 2009
... The Sandvik grade Kanthal APMT is an advanced powder metallurgical resistance heating alloy of the family FeCrAlMo that has good form stability at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2009) 58 (7): SS-1038.
Published: 01 July 2009
... Kanthal APM HP is an advanced high-purity powder metallurgical dispersion-strengthened resistance heating or high-temperature alloy of the family FeCrAlMo that has good form stability at high temperatures. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2009) 58 (11): Fe-149.
Published: 01 November 2009
... Kanthal 180 R05 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 200 deg C (−4 to 390 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (2009) 58 (12): Fe-150.
Published: 01 December 2009
... Kanthal 145 R15 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... KANTHAL 70 alloy was designed to provide a high positive temperature coefficient to electrical resistance comparable with that of pure nickel; however, it has much higher electrical resistivity than pure nickel. This makes it useful as a voltage regulator when placed in series with another...
Journal Articles
Alloy Digest (2010) 59 (7): Fe-151.
Published: 01 July 2010
... Kanthal 135 is a thermostatic bimetal and is recommended for use in the temperature range -20 to 200 deg C (-4 to 572 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code...
Journal Articles
Alloy Digest (2008) 57 (5): Mn-4.
Published: 01 May 2008
... Kanthal 200R10 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (2008) 57 (2): Mn-3.
Published: 01 February 2008
... Kanthal 200/72, a thermostatic bimetal, is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: MN-3. Producer or source: Kanthal AB...
Journal Articles
Alloy Digest (2010) 59 (8): Fe-152.
Published: 01 August 2010
... Kanthal 135 R05 is a thermostatic bimetal and is recommended for use in the temperature range -20 to 250 deg C (-4 to 482 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1136.
Published: 01 February 2013
... as forming. Filing Code: SS-1136. Producer or source: Kanthal AB. Producer or Source: Kanthal AB Copyright © ASM International® 2013 2013 ASM International Alkrothal 720 chemical composition creep properties elasticity hardness high-temperature alloys physical properties resistance wires...
Journal Articles
Alloy Digest (2009) 58 (3): SS-1032.
Published: 01 March 2009
.... Filing Code: SS-1032. Producer or source: Kanthal AB. Producer or Source: Kanthal AB Copyright © ASM International® 2009 2009 ASM International Alkrothal 14 chemical composition creep properties elasticity hardness low-temperature alloys physical properties resistance wires tensile...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1039.
Published: 01 August 2009
... on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: SS-1039. Producer or source: Kanthal AB. Producer or Source: Kanthal AB Copyright © ASM International® 2009 2009 ASM International chemical composition corrosion...