Alloy Digest (2009) 58 (7): SS-1038.
Published: 01 July 2009
... Kanthal APM HP is an advanced high-purity powder metallurgical dispersion-strengthened resistance heating or high-temperature alloy of the family FeCrAlMo that has good form stability at high temperatures. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1997) 46 (8): SS-694.
Published: 01 August 1997
... Kanthal APM is an electric resistance heating alloy based on the iron-chromium-aluminum family. Alloys of this family have longer lives and higher operating temperatures than nickel-chromium alloys. This datasheet provides information on composition, physical properties, hardness, and tensile...