Journal Articles
Alloy Digest (1970) 19 (5): SS-238.
Published: 01 May 1970
... Kanthal A-1 is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. Maximum operating temperature 2505 F (1375 C). This datasheet provides information on composition...
Journal Articles
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... automobile applications chemical composition corrosion-resistant alloys electrical resistance electrical resistivity heat treatability joinability KANTHAL 70 physical properties resistance thermometers tensile properties workability 1 Filing Code: Ni-270 KANTHAL 70 Nickel Alloy 08 SEPTEMBER...
Journal Articles
Alloy Digest (2009) 58 (7): SS-1038.
Published: 01 July 2009
... temperatures. Corrosion Resistance: The maximum recommended operating temperature in air is 1425 °C (2595 °F) to maintain the protective surface oxide of Al2O3. Figure 1 gives weight gain in a cycle test, 900 1300 °C (1650 2370 °F) with time. See also Fig. 2 and 3. General Characteristics: Kanthal APMT...
Journal Articles
Alloy Digest (2008) 57 (8): Mn-5.
Published: 01 August 2008
... Kanthal 200 R 110 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: MN-5...
Journal Articles
Alloy Digest (2009) 58 (6): SS-1037.
Published: 01 June 2009
... operating temperature in air is 1250 °C (2280 °F) to maintain the protective surface oxide of Al2O3. Figure 1 gives weight gain at 1200 °C (2190 °F) with time in a cycling test. General Characteristics: Kanthal APMT is an advanced powder metallurgical, dispersion-strengthened, ferritic FeCrAlMo alloy...
Journal Articles
Alloy Digest (2008) 57 (2): Mn-3.
Published: 01 February 2008
.... Invar is a registered trademark of Imphy Alloys S.A. Temperature range, °C (°F) 10 to 250 (14 to 482) Maximum operating temperature, °C (°F) 330 (626) See also Table 1. Mechanical Properties: Young s modulus, GPa (106 psi) 135 (20) See also Table 2. General Characteristics: Kanthal 200/72...
Journal Articles
Alloy Digest (2008) 57 (10): Fe-147.
Published: 01 October 2008
...-expansion side 155TB1577 Mechanical Properties: Young s modulus, at 20 °C (68 °F), GPa (106 psi) 170 (25) See also Table 1. General Characteristics: Kanthal 155 is a thermostatic bimetal that is recommended for use in the temperature range 20 to +350 °C ( 4 to 660 °F) with extreme case capability...
Journal Articles
Alloy Digest (2009) 58 (11): Fe-149.
Published: 01 November 2009
...) 350 (660) Marking on the high-expansion side 180R05TB1805 Mechanical Properties: Young s modulus, at 20 °C (68 °F), GPa (106 psi) 130 (18.9) See also Table 1. General Characteristics: Kanthal 180 R05 is a thermostatic bimetal recommended for use in the temperature range 20 to 200 °C ( 4 to 390 °F...
Journal Articles
Alloy Digest (2009) 58 (12): Fe-150.
Published: 01 December 2009
... Kanthal 145 R15 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (2010) 59 (7): Fe-151.
Published: 01 July 2010
... °C (68 °F), GPa (106 psi) 170 (24.7) Alloy Designation Portion of thickness, % High-expansive component 22-3 460 50 Low-expansive component Invar 145 50 Intermediate component See Table 1 for additional mechanical properties. General Characteristics: Kanthal 135 is a thermostatic bimetal which...
Journal Articles
Alloy Digest (2008) 57 (5): Mn-4.
Published: 01 May 2008
... Kanthal 200R10 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (2010) 59 (8): Fe-152.
Published: 01 August 2010
... Kanthal 135 R05 is a thermostatic bimetal and is recommended for use in the temperature range -20 to 250 deg C (-4 to 482 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...
Journal Articles
Alloy Digest (1997) 46 (8): SS-694.
Published: 01 August 1997
... 1100 2010 2550 1300 2370 2100 1150 2100 1920 1OSo 1920 2550 l4w 2550 2190 1200 2190 2100 1200 2190 1400 2370 1200 2190 1lsY 2100/ loo0 1830 13cQ 2370 1100 a010 -1 0 100 I 200 300 400 500 600 Tune 0 0 damage heating elements. Chlorine in different forms attack Kanthal. Splashes of molten metal or salt...
Journal Articles
Alloy Digest (1985) 34 (12): Fe-71.
Published: 01 December 1985
... KANTHAL AF is an Fe-Cr-Al alloy intended for heating elements with element temperatures up to 1400 C. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: Fe-71. Producer or source: The Kanthal Corporation. Producer or Source...
Journal Articles
Alloy Digest (1967) 16 (12): SS-203.
Published: 01 December 1967
... 1996 ASM International ceramic kilns chemical composition corrosion-resistant alloys electric heating apparatus fracture toughness furnaces hardness heating elements high-temperature alloys joinability Kanthal-DS physical properties tensile properties I KANTUAI nn1r 1 nnL-DS 111...
Journal Articles
Alloy Digest (1955) 4 (9): SS-34.
Published: 01 September 1955
... KANTHAL-D is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1136.
Published: 01 February 2013
... as forming. Filing Code: SS-1136. Producer or source: Kanthal AB. Producer or Source: Kanthal AB Copyright © ASM International® 2013 2013 ASM International Alkrothal 720 chemical composition creep properties elasticity hardness high-temperature alloys physical properties resistance wires...
Journal Articles
Alloy Digest (1954) 3 (7): SS-16.
Published: 01 July 1954
... International chemical composition corrosion-resistant alloys fracture toughness hardness high-temperature alloys joinability Kanthal-A physical properties tensile properties I I I Filing Coda 5816 !oI DIGEST 1 1 THAL-A Stainlest Steel I JULY, 1954 - DATA ON WORLD WIDE METALS AND ALLOYS KANTHAL...
Journal Articles
Alloy Digest (2010) 59 (6): Cu-784.
Published: 01 June 2010
...: Kanthal Corporation. Producer or Source: Kanthal Corporation Copyright © ASM International® 2010 2010 ASM International chemical composition Cuprothal 49 Cuprothal 49TC electrical resistance hardness physical properties precision resistors tensile properties workability thermal...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1030.
Published: 01 February 2009
... on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming. Filing Code: SS-1030. Producer or source: Kanthal AB. Producer or Source: Kanthal AB Copyright © ASM International® 2009 2009 ASM...