Alloy Digest (2010) 59 (8): Fe-152.
Published: 01 August 2010
... Kanthal 135 R05 is a thermostatic bimetal and is recommended for use in the temperature range -20 to 250 deg C (-4 to 482 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...