Alloy Digest (1959) 8 (8): Cu-79.
Published: 01 August 1959
... KUMANIC is a copper-manganese-nickel alloy that responds to hardening by heat treatment. It has high tensile and fatigue strength along with excellent resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It...