Alloy Digest (2002) 51 (6): Ni-585.
Published: 01 June 2002
... KUBOTA KHR48N HiSi is a Ni-Cr-Fe alloy with a 5% W addition. The alloy was designed for high-temperature operating parameters of strength, good carburization resistance, and high oxidation resistance. It is a modification of KHR48N (see Alloy Digest Ni-582, May 2002) adjusted in composition...
Journal Articles
Alloy Digest (2002) 51 (5): Ni-582.
Published: 01 May 2002
... KUBOTA KHR48N is a Ni-Cr-Fe-W high-carbon alloy with high-temperature operating parameters of strength, good carburization resistance, and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (2002) 51 (9): Ni-591.
Published: 01 September 2002
... Carburization Resistance Alloy Weight gain, mg/mm2 HK 0.33 HP 0.23 KHR48NCo 0.21 KHR48N-HiSi 0.18 ...