Alloy Digest (2007) 56 (11): Ni-655.
Published: 01 November 2007
... strength elasticity hardness heat treatability high-temperature alloys joinability KUBOTA HW machinability physical properties tensile properties thermal properties Chemical Composition, wt Carbon 0.35 0.75 Manganese 2.0 max Silicon 2.5 max Chromium 10 14 Nickel 58 62 Molybdenum 0.5 max...
Journal Articles
Alloy Digest (2008) 57 (1): Ni-658.
Published: 01 January 2008
... Kubota alloy HX is a nickel alloy casting grade with moderate strength, but better oxidation resistance than HW (See Alloy Digest Ni-655, November 2007). The alloy is suitable for service up to approximately 1165 deg C (2125 deg F). This datasheet provides information on composition, physical...