Alloy Digest (2007) 56 (10): SS-998.
Published: 01 October 2007
... Kubota alloys HK40 and HK50 are austenitic Fe-Cr-Ni alloys that have been standard heat-resistant materials for more than four decades. With moderately high temperature strength, oxidation resistance, and carburization resistance the alloys are used in a wide variety of industrial applications. HK...