Alloy Digest (2006) 55 (11): SS-980.
Published: 01 November 2006
... Kubota alloy HH II is a heat-resistant fully austenitic stainless steel casting for multiple furnace parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1999) 48 (3): SS-738.
Published: 01 March 1999
... Kubota alloy KHR12C is an austenitic Fe-Cr-Ni-Nb casting alloy developed from the well known HH type II grade. This alloy is superior to other grades in components that are subjected to frequent thermal cycling and shock. The alloy is available in both centrifugal and static castings...