Skip Nav Destination
Close Modal
Search Results for
KUBOTA ALLOY KHR32C
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
KUBOTA ALLOY KHR32C
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1999) 48 (6): SS-746.
Published: 01 June 1999
... Kubota alloy KHR32C is often regarded as the cast version of Fe-Ni-Cr alloy 800H except it uses niobium as a strengthening agent. The moderately priced alloy has good creep ductility and is available in many cast forms. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Kubota alloy KHR32C is often regarded as the cast version of Fe-Ni-Cr alloy 800H except it uses niobium as a strengthening agent. The moderately priced alloy has good creep ductility and is available in many cast forms. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on casting. Filing Code: SS-746. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (1999) 48 (9): SS-761.
Published: 01 September 1999
... by Kubota. Min Max Carbon 0.18 0.23 Manganese 1.5 Silicon 0.5 1.2 Chromium 24 26 Nickel 36.5 38.5 Phosphorus <0.03 Sulfur <0.03 Niobium 1.5 DOI: 10.31399/asm.ad.ss0761 low-carbon KHR32C alloy, the higher chromium and nickel lev- els in KHR35CL provide greater resistance to oxidation and car...
Abstract
View article
PDF
Kubota alloy KRH35CL is similar to KHR35C but contains lower carbon for applications requiring good thermal fatigue and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-761. Producer or source: Kubota Metal Corporation.