Alloy Digest (1999) 48 (3): SS-738.
Published: 01 March 1999
... Kubota alloy KHR12C is an austenitic Fe-Cr-Ni-Nb casting alloy developed from the well known HH type II grade. This alloy is superior to other grades in components that are subjected to frequent thermal cycling and shock. The alloy is available in both centrifugal and static castings...
Journal Articles
Alloy Digest (2008) 57 (2): SS-1008.
Published: 01 February 2008
... KHR16C was developed from KHR12C (See Alloy Digest SS-738, March 1999), but contains niobium for strength and aged ductility. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1999) 48 (4): SS-740.
Published: 01 April 1999
... Kubota alloy KHR20T is an iron-chromium-nickel cast alloy with microalloying additions that increase its strength to greater than that of HK40 from 871-982 C (1600-1800 F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...