Alloy Digest (2011) 60 (3): SS-1085.
Published: 01 March 2011
... Kubota Alloy CH-20 (ASTM A743) is an iron-chromium-nickel alloy that has other variations with lower carbon and addition of molybdenum. The nearest wrought equivalent is type 309 stainless. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (2011) 60 (2): SS-1082.
Published: 01 February 2011
... Kubota Alloy CK-20 is an iron-chromium-nickel alloy that has other variations with lower carbon and addition of molybdenum. The alloy provides good resistance to dilute sulfuric acid. The nearest wrought equivalent is AISI Type 310 stainless. This datasheet provides information on composition...