Alloy Digest (2016) 65 (12): Cu-854.
Published: 01 December 2016
... Kobelco Alloy SuperKFC has high strength and high conductivity for electronic applications. The alloy is nominally Cu-0.3Fe-0.1P. This datasheet provides information on composition, physical properties, hardness, and tensile properties. and bend strength. It also includes information on forming...