1-1 of 1 Search Results for

KME Cu-DHP

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2021) 70 (8): Cu-923.
Published: 01 August 2021
... KME Cu-DHP is a phosphorus-deoxidized copper that contains a minimum of 99.90% copper and high residual phosphorus. The electrical conductivity of this type of copper is relatively low on account of the high phosphorus content. KME Cu-DHP possesses very good formability and joining properties...