Skip Nav Destination
Close Modal
Search Results for
KIDD ALLOY ZA-27
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for KIDD ALLOY ZA-27
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1982) 31 (9): Zn-39.
Published: 01 September 1982
... KIDD Alloy ZA-27 is a zinc-aluminum-copper high-strength foundry alloy. It is well suited to structural applications, once the exclusive domain of malleable cast iron, bronzes and aluminum. ZA-27 offers an as-sand-cast tensile strength of 58,000 to 64,000 psi at modest cost; also, it can be cast...
Abstract
View articletitled, <span class="search-highlight">KIDD</span> <span class="search-highlight">ALLOY</span> <span class="search-highlight">ZA</span>-<span class="search-highlight">27</span>: Zinc-Base <span class="search-highlight">Alloy</span> for Castings
View
PDF
for article titled, <span class="search-highlight">KIDD</span> <span class="search-highlight">ALLOY</span> <span class="search-highlight">ZA</span>-<span class="search-highlight">27</span>: Zinc-Base <span class="search-highlight">Alloy</span> for Castings
KIDD Alloy ZA-27 is a zinc-aluminum-copper high-strength foundry alloy. It is well suited to structural applications, once the exclusive domain of malleable cast iron, bronzes and aluminum. ZA-27 offers an as-sand-cast tensile strength of 58,000 to 64,000 psi at modest cost; also, it can be cast in cold-chamber machines for better properties than those of conventional die-casting alloys. It is extremely resistant to galling because it has natural lubricity and is thus well suited to bearing and bushing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-39. Producer or source: Kidd Creek Mines Ltd.