Alloy Digest (2004) 53 (10): Ni-623.
Published: 01 October 2004
... Kubota alloy KHRSA is very highly alloyed to produce some of the best strength and oxidation resistance of any of the heat-resisting casting grades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue...
Journal Articles
Alloy Digest (2002) 51 (8): SS-858.
Published: 01 August 2002
... KHR35H 1000 1832 0.30 12 1100 2012 0.81 32 KHR48N 1000 1832 0.22 8.7 1100 2012 0.77 30 KHRSA 1000 1832 0.06 2.4 1100 2012 0.10 3.9 KHRS2 1000 1832 0.26 10 1100 2012 0.37 15 KHRS3 1100 2012 0.23 9.1 DOI: 10.31399/asm.ad.ss0858 Product Forms Available: Static castings and horizontal and vertical...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-598.
Published: 01 December 2002
... subject to periodic revisions as the results from long-term tests become available. Table 3 Comparative Oxidation Rates Temperature Oxidation rate Grade °C °F mm/yr mils/yr KHR35H 1000 1832 0.30 12 1100 2012 0.81 32 KHR48N 1000 1832 0.22 8.7 1100 2012 0.77 30 KHRSA 1000 1832 0.06 2.4 1100 2012 0.10 3.9...