Alloy Digest (2001) 50 (10): Co-108.
Published: 01 October 2001
... KHR40CM is a Co-Cr-Ni-Fe alloy with high-temperature operating parameters of strength, thermal fatigue, and oxidation resistance. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength. It also includes information...
Journal Articles
Alloy Digest (2010) 59 (1): Ni-676.
Published: 01 January 2010
... 0.73 UMCo50 0.55 0.40 4.30 KHR40CM 0.58 1.39 4.25 KNC-01 0.18 0.42 Stress = 4.9 MPa (0.5 kg/mm2), 10,000 cycles Table 5 Vickers hardness at elevated temperature Alloy Vickers hardness (HV) 1000 °C (1832 °F) 1050 °C (1922 °F) 1100 °C (2012 °F) KNC-03 107 101 87 KHR40CM 80 71 62 HK-40 100 90 Prior aging...