Alloy Digest (2017) 66 (8): Cu-863.
Published: 01 August 2017
... treatability joinability KEMPER KHP1 machinability physical properties switchblade jaws tensile properties workability thermal properties UNS C15100 Alloy KHP 151 is a high performance copper alloy with very high conductivity. Chemical Composition, wt (Nominal, maximum) Zirconium 0.05-0.15 Aluminum...