Alloy Digest (2018) 67 (8): Cu-877.
Published: 01 August 2018
... International bend strength chemical composition corrosion-resistant alloys electrical conductivity hardness joinability KEMPER CuSn10 physical properties tensile properties thermal conductivity wear resistance workability UNS C52400 Alloy CuSn10 is a high-performance copper alloy. Chemical...