Alloy Digest (2008) 57 (5): Mn-4.
Published: 01 May 2008
... Kanthal 200R10 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing...