Skip Nav Destination
Close Modal
Search Results for
KAISER aluminum alloy 2124
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
KAISER aluminum alloy 2124
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2008) 57 (5): Al-413.
Published: 01 May 2008
... Kaiser aluminum alloy 2124 is a high-purity version of 2024 with tighter controls on the iron and silicon for an increase in strength and toughness. It is primarily used as plate in the aircraft industry. This data sheet applies to sheet, coil, and plate in the T851 temper. This datasheet provides...
Abstract
View article
PDF
Kaiser aluminum alloy 2124 is a high-purity version of 2024 with tighter controls on the iron and silicon for an increase in strength and toughness. It is primarily used as plate in the aircraft industry. This data sheet applies to sheet, coil, and plate in the T851 temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: AL-413. Producer or source: Tennalum, A Division of Kaiser Aluminum.