Alloy Digest (1963) 12 (4): SA-144.
Published: 01 April 1963
... Jalloy-S is the trade name of a group of constructional steels which combine high strength with welding and forming ease. They are available in three grades according to their minimum yield strength, namely, Jalloy-S-90, Jalloy-S-100, and Jalloy-S-110. This datasheet provides information...
Journal Articles
Alloy Digest (1963) 12 (9): SA-153.
Published: 01 September 1963
...-300 sfpm for carbide tools and 35-60 sfpm for high speed steel tools. The feed should be under 0.015 ipr. Face milling should be done at 400 sfpm with carbide. Using s diameter M-2 high speed steel drills and a feed of 0.002 ipr, good drill life can be obtained at cutting speeds of 60-120 ft/min...
Journal Articles
Alloy Digest (1957) 6 (11): SA-3.
Published: 01 November 1957
... msr. siIicon O.lM.30 MOl+dCfllUB 0.10430 Iron PROPERTIES T&l.1 TYPICAL HOT-ROLLED pROPERTIES-BARS condirion As-rolled Srress relief 1OOO F Stress relief llOO°F Stress relief 1200°F Scnss relief 13OO F Normalid 1625°F Aonded 1600°F Yield Tensile S-M S-grh pai pri E 80000 78 57000 82000 58000 81000...