Alloy Digest (2005) 54 (1): Fe-135.
Published: 01 January 2005
... JNHF-Core is a chemical vapor deposition (CVD) processed, nonoriented, high-silicon soft magnetic steel sheet that has a silicon density gradient of between 3 to 6.5 wt.%. The silicon steel sheet consists of three gradated silicon density areas, a high-Si area, a low-Si area, and another high-Si...