Alloy Digest (1968) 17 (5): SA-226.
Published: 01 May 1968
... JLX-50CC is a high-strength columbium steel designed for ease of fabrication. It has good formability, weldability, and toughness. It is recommended for mining equipment, automobile and truck bodies, trailers and similar construction. This datasheet provides information on composition, physical...