Alloy Digest (1959) 8 (3): SS-85.
Published: 01 March 1959
... JETHETE M.160 is a 12% chromium air hardening alloy steel having high resistance to stress-corrosion cracking. It is recommended for use at temperatures approaching 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1961) 10 (4): SS-116.
Published: 01 April 1961
... Jethete M.151 is a high strength, transformable stainless steel, suitable for welding. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on forming, heat treating, and joining. Filing Code: SS...