1-20 of 29 Search Results for

JESSOP no. 200

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1960) 9 (6): SA-99.
Published: 01 June 1960
... JESSOP No. 200 is a non-magnetic, austenitic steel developed especially for the electrical industry. It has low magnetic permeability and high electrical resistance. Jessop No. 200 is ideal for a great number of applications requiring low permeability material where corrosion resistance is not a...
Journal Articles
Alloy Digest (1963) 12 (12): SA-158.
Published: 01 December 1963
... Jessop No. 9 is a non-magnetic super high tensile steel having exceptionally high toughness and wear resistance. It is recommended for heavy earth moving equipment subject to severe battering. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (1957) 6 (6): Ni-35.
Published: 01 June 1957
... alkaline solutions it has excellent resistance to corrosion. It has useful resistance to mol- ten lead but not to other low-melting point metals. General Characteristics: Jessop G.39 is an austenitic nickel-base alloy inrended for use in the as-cast condition with no subsequent heat treatment. It has...
Journal Articles
Alloy Digest (1965) 14 (3): Zr-2.
Published: 01 March 1965
... JESSOP-SAVILLE ZIRCONIUM Alloy has a high melting point and possesses excellent corrosion resistance coupled with low neutron absorption properties. It is equivalent to ZIRCALOY 2. It is recommended for pressurized water reactors. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (10): Ni-293.
Published: 01 October 1983
... Equivalents: UNS No. N08825. ASTM B 424. General Characteristics: As mentioned in the introduction, Jessop JS825 is a nickel-iron-chromium-molybdenum-copper alloy for use in extremely corrosive environments. It is a wrought material and is used normally in the annealed (solution-treated) condition; however...
Journal Articles
Alloy Digest (1984) 33 (6): SS-448.
Published: 01 June 1984
... JESSOP JS800/800H is an austenitic stainless steel with good resistance to corrosion and oxidation at elevated temperatures; 800 and 800H are identical in composition except that 800H contains a higher specified level of carbon than 800. This steel also shows fair resistance to stress-corrosion...
Journal Articles
Alloy Digest (1986) 35 (8): Ni-337.
Published: 01 August 1986
... JESSOP ALLOY G is a nickel-chromium-iron-molybdenum-copper alloy exhibiting excellent resistance to a variety of corrosive conditions. It is resistant to both alkaline and acid environments, to stress-corrosion and to hot flue gases. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (7): TS-195.
Published: 01 July 1967
... Jessop-Saville JO. Special is a basic hot work tool steel exhibiting good red-hardness and abrasion resistance at elevated temperatures. It is recommended for forging and extrusion dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1983) 32 (4): Ni-285.
Published: 01 April 1983
... JESSOP JS625 is a nickel-chromium-molybdenum-columbium alloy that is well suited for applications where strength and corrosion resistance are required. It has superior strength and toughness at temperatures ranging from cryogenic to 2000 F; also, it has exceptional fatigue strength. It is...
Journal Articles
Alloy Digest (1984) 33 (2): SS-440.
Published: 01 February 1984
.... Elecrropolishlng is satisiactorb. Specification Equivalents: UNS No. S 17700. ASTM A 693. General Characteristics: As mentioned m the introducrlon. Jessop JSlTCr-7Ni IS a semi- austeniric. preclpnation-hardeningsreel: It contains lchromium. 7pc nickel and I? aluminum The chemlsrr) of this alloy gives II a unique...
Journal Articles
Alloy Digest (1982) 31 (7): SS-412.
Published: 01 July 1982
... JESSOP JS17Cr-4Ni is a martensitic, precipitation-hardening chromium-nickel-copper stainless steel. It provides an excellent combination of high strength and hardness, short-time low-temperature precipitation hardening and good mechanical properties at temperatures up to 600 F (316 C). Its...
Journal Articles
Alloy Digest (1981) 30 (3): TS-378.
Published: 01 March 1981
... 178-200 l/32 151-170 Sulphurized mineral oiI is recommended as the cut- ting fluid for turning, boring, shaping, and planing; while soluble cutting oil is recommended for grind- ing and high-speed sawing. Hardened Jessop BX3 steel is relatively difficult to grind because of its extreme resistance to...
Journal Articles
Alloy Digest (1983) 32 (8): Ni-289.
Published: 01 August 1983
... by using a vacuum or very dry hydrogen. In general, it must be pickled to obtain a bright surface. The alloy manufacturer can provide details on pickling. Specification Equivalents: UNS No. NO6007. ASTM B 582 General Characteristics: As mentioned in the introduction, Jessop JS Alloy G is a nickel...
Journal Articles
Alloy Digest (1983) 32 (6): Ni-287.
Published: 01 June 1983
.... Details for pickling are available from the manufacturer. Specification Equivalents: ASTM B 168. UNS No. N06600. Generai Characteristics: As stated in the introduction, Jessop JS600 is a nickel- chromium-iron alloy for use in environments requiring resistance to heat and corrosion. The high nickel content...
Journal Articles
Alloy Digest (1987) 36 (5): Ni-348.
Published: 01 May 1987
.... Specification Equivalents: ASTM B 582. ASME SB 582. UNS No. N06985. General Characteristics: JESSOP JS alloy G-3 is readily fabricable, hot or coM, and it has excellent weldability with minimal loss of heat-affected zone corrosion resistance after welding. It has outstanding resistance to pitting and gcaeral...
Journal Articles
Alloy Digest (1982) 31 (11): SS-416.
Published: 01 November 1982
... taken if welded in this condition. Specification Equivalents: ASTM A 693. UNS No. Sl5500. General Characteristics: As mentioned in the introduction, Jessop JSISCr-5Ni is a marten- sitic. precipitation-hardening stainless steel. It is characterized by high hardness and strength along with good corrosion...
Journal Articles
Alloy Digest (1963) 12 (6): Co-21.
Published: 01 June 1963
... JESSOP-SAVILLE G.32 is a cobalt-base alloy having high oxidation and corrosion resistance. It is recommended for high temperature applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep...
Journal Articles
Alloy Digest (1983) 32 (12): TS-419.
Published: 01 December 1983
... welding methods necessary, but again the principle of adequate preheating and slow cooling should be respected to minimize risks. Specification Equivalents: AISI Type H 13. SAE Type H 13. UNS No. T20813. General Characteristics: Jessop Dica B Vanadium is an air-hardening hot-work tool steel that is used...
Journal Articles
Alloy Digest (1984) 33 (4): TS-422.
Published: 01 April 1984
... Feed High-Speed Cemented inch in. /rev. Steel Carbide 1132 1,164 58-66 240-280 Ii16 l/32 48-54 200-230 118 l/32 4@46 18Gl95 l/4 Ii32 34-38 150-170 Workability: Jessop Supershock 7 can be hot forged or hot rolled readily. Heat slowly and uniformly to 1800~1950°F. Do not forge below 16OO F. Reheat if...
Journal Articles
Alloy Digest (1955) 4 (5): TS-33.
Published: 01 May 1955
... hardening. General Characteristics: Jessop 2-B (L.C.) ls a low carbon, medium tungsten hoc work steel Little or no reduction in hardness is obsuped in hot operations up co approximately 1100 deg. F. Deformation is minimized because of the ex- cellent air hardening properties. It is possible co ob- tain a...