... JESSOP TYPE 316L is an extra low carbon variation of Jessop TYPE 316 (See Alloy Digest SS-488, August 1987). It is formulated for resistance to intergranular corrosion in welded or stress relieved structures. JESSOP TYPE 316LM is a more highly alloyed modification of 316L (higher molybdenum and...
Journal Articles
Alloy Digest (1989) 38 (1): SS-502.
Published: 01 January 1989
... crevice corrosion resistance, a contribution mainly of their molyb- denum content General Characteristics: JESSOP TYPE 317L and 317L Plus have superior cor- rosion resistance, high-temperature strength, stress-rup- ture and creep resistance compared to AISI type 316L. Resistance to pitting and crevice...