Alloy Digest (1984) 33 (2): SS-440.
Published: 01 February 1984
... JESSOP JS17Cr-7Ni is a semi-austenitic precipitation-hardening steel. Its composition gives it a unique and attractive combination of corrosion resistance, cold formability, high strength and hardness, excellent fatigue properties and minimum distortion upon heat treatment. Typical applications...